- On structural phase transitions in 4-aminopyridinium fluoroborate, [4-NH²C5H5N][BF4] : differential scanning calorimetry, dielectric and infrared studies
Description
- Title: On structural phase transitions in 4-aminopyridinium fluoroborate, [4-NH²C5H5N][BF4] : differential scanning calorimetry, dielectric and infrared studies
- Journal title: Journal of Molecular Structure
- Creator: Czupiński, Olaf ; Jakubas, Ryszard ; Pietraszko, A
- Pages: s. 177-187
- Description: Zawiera wykresy. ; Zawiera ilustracje. ; Bibliogr. ; Streszcz. w jęz. ang.
- Language of abstract: eng
- Date issued: 2004
- Type: Tekst
- Language: eng
- Detailed object type: art
- Object type: Artykuł
- Location: Vol. 704 (2004), s. 177-187 : il.